4 Mortar hollowing problem 1. Constructive hollowing The roughness of the interface agent is insufficient or the plaster layer is loosened due to rubbing and pressing before the mortar is collected. Or the mortar itself has insufficient bonding strength. Cause peeling between the mortar layer and the interface agent layer. 2. Shrinkage empty drum The

Five major quality problems of wet-mixed mortar and their solutions(1)

By |2023-05-10T02:36:57+00:00May 9th, 2023|Industry News|

1. The drying time of plastering mortar on the wall The drying time on the wall is mainly related to four aspects: the degree of water absorption of the wall, the water retention of the mortar, the setting time of the mortar, and the ambient humidity. 1. The wall humidity is normal and the air